Description
ITEM | GB/T4100-2006 Appendix G GB REQUIRED STANDARDS |
HUIDA STANDARDS |
---|---|---|
The diviation of the average size for each tile (2 sides) from the work size |
±0.5 n=10, Ac=0,,Re=2 |
-0.08~+0.06 d=0 |
The diviation in percent of the average size for each tile(2 sides) from the average size of the 10 test specimens(20 sides) |
±0.4 n=10, Ac=0,,Re=2 |
-0.01~+0.02 d=0 |
Thickness | ±5 n=10, Ac=0,,Re=2 |
-1.0~+2.6 d=0 |
Staightness | ±0.3 n=10, Ac=0,,Re=2 |
-0.02~+0.01 d=0 |
Wedging | ±0.5 n=10, Ac=0,,Re=2 |
-0.07~+0.04 d=0 |
Central Bending Strenght(%) | ±0.4 n=10, Ac=0,,Re=2 |
-0.02~+0.02 d=0 |
Edge Bending Strenght(%) | ±0.4 n=10, Ac=0,,Re=2 |
-0.05~+0.03 d=0 |
Surface Quality | a minimum of 95% of the tiles shall be free from visible defects that would impair the appearance of a major area of tiles n=5, Ac=0,,Re=2 |
no visible defects d=0 |
Water Absorption | average:E≤1 individual:E≤1 n=5, Ac=0,,Re=2 |
average:1 individual maximum:1 d=0 |
Disruptive Strenght | thickness≥7.5mm,≥1300N thickness≤7.5mm,≥700N n=5, Ac=0,,Re=2 |
average value:3007 d=0 |
Broken Value(Mpa) | average value:≥35MPa individual:≥32MPa n=5, Ac=0,,Re=2 |
average value:43 minimum value:42 d=0 |
Abrasion Resistance | report abrasion class and cycles passed |
3 class(1500 cycles) |
Thermal Expantion Coeeficent |
no crack or crazing after test n=5, Ac=0,,Re=2 |
no crack or crazing d=0 |
Frost Resistance | no crack or crazing after test n=10, Ac=0,,Re=2 |
no crack or crazing after test d=0 |
Cracking Glaze Strenght |
no crazing on glazed surface after test n=5, Ac=0,,Re=2 |
no crazing d=0 |
Dirt Resistance |
minimum class 3 n=5, Ac=0,,Re=2 |
5 d=0 |
Resistance to household chemicalsand swimming pool salts |
minimum GB n=5, Ac=0,,Re=2 |
GA d=0 |
Resistance to low concentrations of acids and alkalis |
GLA、GLB、GLC | GLA |
Resistance to high concentrations of acids and alkalis |
GHA、GHB、GHC | GHA |